WebDec 29, 2011 · The method of chloridizing roasting-leaching method purifying silicon dioxide ore is the application of dchlorine metallurgy principle, and this method has the … WebThe chloridizing of stibnite with calcium chloride was studied as an alternative to volatilize antimony from impure copper concentrates because the vapor pressure of antimony chloride is higher than the vapor pressures of antimony oxide or sulfide at low temperatures. ... the chloridizing roasting of Sb2S3 using CaCl2–O2 was investigated to ...
Roasting chloridizing - Big Chemical Encyclopedia
WebRoasting of Chalcocite (Cu 2 S) to obtain Copper Oxide (Cu 2 O). 2Cu 2 S + 3O 2 → 2Cu 2 O + 2SO 2. Conversion of metal compounds to chlorides through Chloridizing Roasting. 2NaCl + MS + 2O 2 → Na 2 SO 4 + MCl, 4NaCl + 2MO + S 2 + 3O 2 → 2Na 2 SO 4 + 2MCl 2. Controlled roasting of a non-magnetic ore like haematite to convert it into ... WebFeb 7, 2024 · A key step in the ferronickel production process is sulfate-chloridizing roasting. At this stage, highly volatile chlorides and (or) metal oxychlorides under certain conditions are transferred to the gas phase (chloride sublimation) for subsequent separation and obtaining high-purity materials. installing faucet in bathtub
Multiple Hearth Furnace Applications - Industrial Furnace …
WebA chloridizing roast is a roast which, beginning with oxidation, ends by leaving, as nearly as possible, all the silver in the form of chloride in the ore. Scale; 1/4 inch = 1 foot. a.First hearth. b. Second hearth. c.Fire place. … WebThis paper describes a chloridizing roasting process applied to two types of nickel and copper-bearing sulfide concentrates. One was copper rich and the other nickel rich. The … WebA variety of chloridizing agents were admixed with EAF dust to promote the selective removal of lead and cadmium by the formation of volatile metal chlorides. The results of the experimentation firmly establish that selective chloridizing roasting is a technically feasible means of eliminating lead and cadmium from EAF dust. jiffy lube high mileage oil change